Barium Magnetic Ferrite Ring Magnet
Sintered ferrite magnetic ring can not only ordinary charge magnetic (axial radial 1 pair of pole charged magnetic), but also multipole magnetic magnetic, that is, a plane or side multiple poles, we call it multipole magnetic ring, because this product is a sintering process, so also called sintering ferrite multipole magnetic ring.
- MGC
- Ma'anshan City, Anhui Province
- According to customer order quantity
- 10,000 tons/year
- Information
Sintered ferrite magnetic ring can not only ordinary charge magnetic (axial radial 1 pair of pole charged magnetic), but also multipole magnetic magnetic, that is, a plane or side multiple poles, we call it multipole magnetic ring, because this product is a sintering process, so also called sintering ferrite multipole magnetic ring.
Sintered ferrites (also known as ceramic magnets) were developed and produced in the 1950's;
Sintered ferrite magnets mainly include barium ferrite (BaO•6Fe2O3) and strontium ferrite (SrO•6Fe2O3); sintered ferrite is divided into isotropic magnets and anisotropic magnets.
Performance: The magnetic properties of isotropic sintered ferrite are weak, and have the same magnetic properties in any direction.
Multi-pole magnetization in any direction; Anisotropic sintered ferrite magnets have higher magnetic properties than isotropic ones,
It can only be magnetized in the orientation direction of the magnetic field during molding; the main raw material of sintered ferrite is oxide,
Therefore, it will not be corroded by high temperature, high humidity or chemical substances (except strong acid and alkali).
Application field: Because the raw materials are cheap and the production process is relatively simple, the cost is low,
Therefore, sintered ferrite is by far the most widely used permanent magnet material;
It is widely used in permanent magnet motors, DC motors, speakers, reed switches, magnetic separators and adsorption devices, etc.
Others: sintered ferrite has excellent demagnetization resistance, no magnetic flux loss before and after assembly and magnetization;
The working temperature of sintered ferrite is -40°C to +250°C, and the temperature coefficient is poor;
The temperature coefficient of Br is -0.2%/°C, that is, for every 1°C increase in temperature, Br decreases by 0.2%;
Sintered ferrite has high hardness and can be processed by wire cutting and grinding;
Sintered ferrite is brittle and fragile, so it should be handled with care during production and transportation.
FAQ
Q:What is the difference between the product performance of the different materials?
A:The common performance of general car starters is MGC 36h, MGC 37h series; the common performance of air conditioners and refrigerators is MGC 35b, MGC 36b series; the common performance of electric tools and ceiling fans is MGC 33, MGC35 series (MGC is our company's magnetic tile grade)
Q:How long is the regular production delivery period after the formal mass production?
A:Generally 25 days, delivered by order delivery.
Q:What if there is no conforming mold for the first product?
A:If there is no conforming mold, a new mold needs to be opened first. The production cycle of the new mold is 20-25 days. The product production can be carried out after the mold production is completed and verified.
Q:Is there any requirement for the product order quantity?
A:Generally there is a minimum starting quantity, a single batch of value in about 10,000-20,000.